- Mechanical Properties
Value Units Test Method / Conditions Tensile Strength 4.4 (636) MPa (psi) ASTM D412 Modulus (100% Elongation) 1.3 MPa ASTM D412 Hardness 40 Shore A ASTM D2240 Tear Strength 116 kN/m ASTM D 624 Elongation 469 % ASTM D412 - Physical Properties
Value Units Test Method / Conditions Density 0.96 g/cm3 ASTM D1505 - Processing Parameters
Value Units Test Method / Conditions Front Temperature 216 - 266 °C - Mold Temperature 27 - 49 °C - Nozzle Temperature 227 - 277 °C - Rear Temperature 210 - 216 °C - Injection Rate 25 - 127 mm/se - Back Pressure 0.52 - 1.21 MPa -