Properties
- Specifications
Value Units Test Method / Conditions Density 1.2 g/cm3 D792 Tensile Strength 45.0 MPa D638 Flexural Strength 80.0 MPa D790 Flexural Modulus 3000.0 MPa D790 Notched Charpy Impact Strength 15.0 KJ/m2 D256 Hardness,Rockwell 103.0 HRR - Heat Deflection Temperature (1.82MPa) 105.0 ℃ D648 Flame Resistance Properties V-0 3.2mm UL-94 Melt Index 3.0 g/10min D1238 Volume Resistivity 1014.0 Ω.cm D257 Molding Shrinkage 0.4-0.6 % D955
Technical Details & Test Data
- Heat Resistance, Heat-resistance Flame Retardant ABS Processing Conditions
Injection temperature 200~225℃, mold temperature 40-80℃,injection pressure 60-90MPa, eliminate moisture at 80-85 ℃ for 2-3 hours.