- Specifications
Value Units Test Method / Conditions Density 1.18 g/cm3 D792 Tensile Strength 38.0 MPa D638 Tensile Elongation 15.0 % D638 Flexural Strength 62.0 MPa D790 Flexural Modulus 2370.0 MPa D790 Notched Charpy Impact Strength 12.0 KJ/m2 D256 Hardness,Rockwell 99.2 HRR - Heat Deflection Temperature (1.82MPa) 90.2 ℃ D648 Flame Resistance Properties V-0 3.2mm UL-94 Melt Index 2.2 g/10min D1238 Volume Resistivity 1014.0 Ω.cm D257 Molding Shrinkage 0.4-0.6 % D955
Technical Details & Test Data
- Flame Retardant PP Processing Conditions
Injection temperature 195~225℃, mold temperature 40-80℃,injection pressure 60-90MPa, eliminate moisture at 80-85 ℃ for 2-3 hours.