Taroprene™ 1A80 M1N

Brand: Taroprene (42 products)

Polymer Name: Thermoplastic Vulcanizate (TPV)

Processing Methods: Injection Molding

Density: 960.0 - 960.0 kg/m³

Tear Strength: 36.0 - 36.0 kN/m

Compression Set (70 °C): 38.0 - 38.0 %

Enhanced TDS

Knowde-enriched technical product data sheet

Identification & Functionality

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Physical Form
Mechanical Properties
ValueUnitsTest Method / Conditions
Hardness80Shore AISO 7619-1
Modulus at 300% Elongation5.9MPaASTM D 412
Modulus at 100% Elongation4.7MPaASTM D 412
Compression Set (22 hr at 158°F)38%ASTM D 395
Tear Strength36kN/mISO 34-1
Physical Properties
ValueUnitsTest Method / Conditions
Melt Flow Index - MFI (190°C/5 kg)3g/10 minASTM D 1238
Density960kg/m3ASTM D 792

Regulatory & Compliance

Packaging & Availability

Regional Availability
  • Europe