Mechanical Properties
ValueUnitsTest Method / Conditions
Hardness50Shore AASTM D 2240
Modulus at 100% Elongation1.4MPaASTM D 412
Modulus at 300% Elongation2.8MPaASTM D 412
Compression Set (22 hr at 158°F)30%ASTM D 395
Tear Strength17kN/mASTM D 624
Physical Properties
ValueUnitsTest Method / Conditions
Melt Flow Index - MFI (190°C/5 kg)2.5g/10 minISO 1133
Density960kg/m3ASTM D 792