Enhanced TDS
Knowde-enriched technical product data sheet
Identification & Functionality
- Additives Included
- Chemical Family
- Polymer Name
- Composite Materials Functions
- Plastics & Elastomers Functions
- Technologies
- Product Families
- Processing Method
Injection Molding
- Additive
Flame Retardant
Features & Benefits
- Labeling Claims
- Materials Features
- Features
- Bromine Free
- Chlorine Free
- Flame Retardant
- Medium Heat Resistance
- Self Extinguishing
Applications & Uses
- Markets
- Applications
- Plastics & Elastomers End Uses
- Composites Processing Methods
- Plastics & Elastomers Processing Methods
Properties
- Physical Form
- Physical Properties
Value Units Test Method / Conditions Density 1.09 - ASTM D792 Melt Mass Flow Rate (at 250°C, 11.6 kg) 20 - 40 g/10 min ASTM D1238 Molding Shrinkage (at 0.125 in, Flow) 5.0E-3 to 7.0E-3 in/in ASTM D955 Molding Shrinkage (at 0.125 in, Across Flow) 5.0E-3 to 7.0E-3 in/in ASTM D955 Specific Gravity 1.09 - ASTM D792 - Mechanical Properties
Value Units Test Method / Conditions Tensile Strength (at Yield, 0.125 in) 8200 psi ASTM D638 Tensile Strength (at Break, 0.125 in) 7100 psi ASTM D638 Tensile Elongation (at Yield, 0.125 in) 6 % ASTM D638 Tensile Elongation (at Break, 0.125 in) 25 % ASTM D638 Flexural Modulus (at 0.125 in) 350000 psi ASTM D790 Flexural Strength (at 0.125 in) 12000 psi ASTM D790 - Thermal Properties
Value Units Test Method / Conditions Deflection Temperature Under Load (at 66 psi, 0.125 in, Unannealed) 210 °F ASTM D648 Deflection Temperature Under Load (at 264 psi, 0.125 in, Unannealed) 200 °F ASTM D648 Relative Thermal Index Electrical Property (at 0.12 in) 149 °F UL 746 Relative Thermal Index Electrical Property (at 0.24 in) 149 °F UL 746 Relative Thermal Index Impact Property (at 0.12 in) 149 °F UL 746 Relative Thermal Index Impact Property (at 0.24 in) 149 °F UL 746 Relative Thermal Index Strength Property (at 0.12 in) 149 °F UL 746 Relative Thermal Index Strength Property (at 0.24 in) 149 °F UL 746 - Electrical Properties
Value Units Test Method / Conditions Volume Resistivity 31000000000000000 ohms·cm ASTM D257 - Flammability
Value Units Test Method / Conditions Flame Rating (at 0.12 in, All) V-1 - UL 94 Flame Rating (at 0.24 in, All) V-1 - UL 94 - Processing Information (Injection Molding)
Value Units Test Method / Conditions Drying Temperature 170 - 180 °F - Drying Time 3.0 - 4.0 hr - Front Temperature 460 - 530 °F - Middle Temperature 440 - 520 °F - Mold Temperature 130 - 170 °F - Rear Temperature 420 - 510 °F - Maximum Drying Time 8 hr - Processing Temperature (Melt) 480 - 530 °F - - Impact Properties
Value Units Test Method / Conditions Impact Strength (at 73°F, Notched Charpy) 8 ft·lb/in² ISO 179/1 Gardner Impact Strength (at 0.125 in) 150 in·lb ASTM D3029 Impact Strength (at -22°F, 0.125 in, Notched Izod) 2 ft·lb/in ASTM D256 Impact Strength (at 73°F, 0.125 in, Notched Izod) 5 ft·lb/in ASTM D256