Enhanced TDS
Knowde-enriched technical product data sheet
Identification & Functionality
- Additives Included
- Chemical Family
- Polymer Name
- Plastics & Elastomers Functions
- Technologies
- Product Families
- Processing Method
Injection Molding
- Additive
UV Stabilizer
Features & Benefits
- Materials Features
- Features
- General Purpose
- Medium Impact Resistance
- UV Resistant
Applications & Uses
- Markets
- Applications
- Plastics & Elastomers End Uses
- Plastics & Elastomers Processing Methods
- Uses
General Purpose
Properties
- Physical Form
- Physical Properties
Value Units Test Method / Conditions Density 1.05 - ASTM D792 Melt Mass Flow Rate (at 230°C, 3.8 kg) 3.0 - 14 g/10 min ASTM D1238 Molding Shrinkage (at 0.125 in, Flow) 5.0E-3 to 7.0E-3 in/in ASTM D955 Specific Gravity 1.05 - ASTM D792 - Mechanical Properties
Value Units Test Method / Conditions Tensile Modulus (at 0.125 in) 380000 psi ASTM D638 Tensile Strength (at Yield, 0.125 in) 7000 psi ASTM D638 Tensile Strength (at Break, 0.125 in) 6000 psi ASTM D638 Tensile Elongation (at Yield, 0.125 in) 2 % ASTM D638 Tensile Elongation (at Break, 0.125 in) 30 % ASTM D638 Flexural Modulus (at 0.125 in) 350000 psi ASTM D790 Flexural Strength (at 0.125 in) 9300 psi ASTM D790 - Thermal Properties
Value Units Test Method / Conditions Deflection Temperature Under Load (at 66 psi, 0.125 in, Unannealed) 190 °F ASTM D648 Deflection Temperature Under Load (at 264 psi, 0.125 in, Unannealed) 180 °F ASTM D648 Relative Thermal Index Electrical Property (at 0.06 in) 140 °F UL 746 Relative Thermal Index Electrical Property (at 0.12 in) 140 °F UL 746 Relative Thermal Index Impact Property (at 0.06 in) 140 °F UL 746 Relative Thermal Index Impact Property (at 0.12 in) 140 °F UL 746 Relative Thermal Index Strength Property (at 0.06 in) 140 °F UL 746 Relative Thermal Index Strength Property (at 0.12 in) 140 °F UL 746 Vicat Softening Temperature 210 °F ASTM D1525 ² - Electrical Properties
Value Units Test Method / Conditions Volume Resistivity 10000000000000000 ohms·cm ASTM D257 - Flammability
Value Units Test Method / Conditions Flame Rating (at 0.06 in, All) HB - UL 94 Flame Rating (at 0.12 in, All) HB - UL 94 - Processing Information (Injection Molding)
Value Units Test Method / Conditions Drying Temperature 180 - 200 °F - Drying Time 3.0 - 4.0 hr - Front Temperature 420 - 460 °F - Middle Temperature 400 - 440 °F - Mold Temperature 120 - 160 °F - Rear Temperature 370 - 410 °F - Maximum Drying Time 8 hr - Processing Temperature (Melt) 425 - 500 °F - - Impact Properties
Value Units Test Method / Conditions Impact Strength (at 73°F, Notched Charpy) 9 ft·lb/in² ISO 179/1eA Impact Strength (at -40°F, 0.125 in, Notched Izod) 1 ft·lb/in ASTM D256 Impact Strength (at 73°F, 0.125 in, Notched Izod) 4 ft·lb/in ASTM D256 Impact Strength (at -22°F, Notched Izod) 3.5 ft·lb/in² ISO 180/1A Impact Strength (at 73°F, Notched Izod) 7.8 ft·lb/in² ISO 180/1A Gardner Impact Strength (at 0.125 in) 200 in·lb ASTM D3029 - Hardness
Value Units Test Method / Conditions Rockwell Hardness (R-Scale) 110 - ASTM D785