Enhanced TDS
Knowde-enriched technical product data sheet
Identification & Functionality
- Additives Included
- Chemical Family
- Polymer Name
- Plastics & Elastomers Functions
- Technologies
- Product Families
Features & Benefits
- Materials Features
Applications & Uses
- Markets
- Applications
- Plastics & Elastomers End Uses
- Plastics & Elastomers Processing Methods
Properties
- Mechanical Properties
Value Units Test Method / Conditions Tensile Strength 25 MPa ISO 7619-1 Tensile Modulus 2200 MPa ISO 527 Flexural Strength 35 MPa ASTM D 790 Flexural Modulus 1700 MPa ASTM D 790 Charpy Notched Impact Strength (23°C) 3 kJ/m2 ISO 179/1eA Charpy Notched Impact Strength (-20°C) 1 kJ/m2 ISO 179/1eA Charpy Impact Strength (23°C) 90 kJ/m2 STN EN ISO 179 Charpy Impact Strength (-20°C) 15 kJ/m2 STN EN ISO 179 Elongation 10 % ASTM D638 - Physical Properties
Value Units Test Method / Conditions Melt Mass Flow Rate - MFR (230°C/2.16 kg) 25 g/10 min ASTM D1238 Density 0.99 g/cm3 ISO 1183 - Thermal Properties
Value Units Test Method / Conditions Heat Deflection Temperature - HDT 90 °C ASTM D648 Melting Temperature (DSC) 160 °C STN EN ISO 11357-1 Vicat Softening Temperature (B) 150 °C STN EN ISO 306 - Electrical Properties
Value Units Test Method / Conditions Surface Resistivity 1.0e+16 ohm ASTM D257 Electric Strength 26 kV/mm IEC 60243-1 Comparative Tracking Index - CTI (A) 450 V STN EN 60112 Volume Resistivity 100000000000000.0 ohm.m ASTM D 257 - Flammability
Value Units Test Method / Conditions Flammability (1.6 mm) V2 -- UL – 94 Glow Wire Test (3 mm) 960 °C STN EN 60695-2-12 - Processing Parameters
Value Units Test Method / Conditions Mold Temperature Range 30 - 50 °C -- Manufacturing Shrinkage - length/width 2.18/1.97 % STN EN ISO 294-4 Melt Temperature Range 200 - 250 °C -- Injection Pressure 50 - 80 MPa --