Extrulen® UHMW-PE Extruded 1020 is distinguished by its exceptional features, including remarkably high notched impact strength, the capability to absorb high energy under elevated stress rates, excellent wear resistance, and a low coefficient of friction. These qualities make it a top-performing material for meeting critical performance criteria in demanding industrial or engineering applications.

Polymer Name: Ultra High Molecular Weight Polyethylene (UHMWPE)

Physical Form: Custom

Features: Crosslinkable, Enhanced Physical Properties, Good Mechanical Properties, Good Notched Impact Strength, High Energy Absorption, Low Coefficient of Friction, Wear Resistant

Density: 936.0 - 936.0 kg/m³

Message our experts with questions
Mark Zuber avatar

Mark Zuber

Technical Sales

Please reach out to me with any questions about our Advanced Materials products in the AMERICAS region: Acetron, Altron PC, Duratron, Ertacetal, Ertalon PA, Ertalyte PET, Fluorosint PTFE, GMTex, Ketron PEEK, Kyron, KyronMAX, Nylatron PA, Semitron, Sterra, Sultron, SymaLITE, Techtron PPS

Cihan Kundakci avatar

Cihan Kundakci

Technical Sales

Please reach out to me with any questions about our Advanced Materials products in the EMEA region: Acetron, Altron PC, Duratron, Ertacetal, Ertalon PA, Ertalyte PET, Fluorosint PTFE, GMTex, Ketron PEEK, Kyron, KyronMAX, Nylatron PA, Semitron, Sterra, Sultron, SymaLITE, Techtron PPS

Knowde Enhanced TDS

Identification & Functionality

Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers End Uses
Plastics & Elastomers Processing Methods

Properties

Physical Form
Mechanical Properties
ValueUnitsTest Method / Conditions
Density (Annealed material)936.0kg/m³ASTM D792 / ASTM D1505
Tensile Stress at Yield (Tensile strength)23MPaASTM F648 / ASTM D638
Tensile Stress at Break (Ultimate tensile strength)56MPaASTM F648 / ASTM D638
Elongation (at Break)467.0%ASTM F648 / ASTM D638
Shore Hardness (15 sec)66.0D - ScaleASTM D2240
Notched Impact Strength (Charpy)187kJ/m²ISO 11542.2
Crystallinity (1ˢᵗ heat, 20°C - 160°C)58.0%ASTM F2625, Differential Scanning Calorimeter
Notched Impact Strength (lzod)148kJ/m²ASTM F648
Water Absorption (at 23°C until Saturation)max. 0.05%ASTM D570
Thermal Properties
ValueUnitsTest Method / Conditions
Melting Temperature (10°C/min)138.0°CASTM DF2625, Differential Scanning Calorimeter
Vicat Softening Point (10N, at 50°C/hr)134.0°CASTM D1525
Coefficient of Linear Thermal Expansion (23°C to 80°C)1.8 x 10⁻⁴K⁻¹ASTM D696
Heat Deflection Temperature (at 1.8 MPa)42.0°CASTM D648
Thermal Conductivityapprox. 0.4W/(m*K)DIN 52612
Crystallization Temperature Range (20°C - 160°C)126 - 144°CASTM F2625
Ash Particlesmax. 150mg/kgISO 3451 -1
Oxidation Resistance (Surface oxidation index)max. 0.1ASTM F2102
Oxidation Resistance (Bulk oxidation index)max. 0.1ASTM F2102
Oxidation Induction Time to Conducted (at 200°C)10.0minASTM D3895