Value Units Test Method / Conditions Density (Annealed material) 935.0 kg/m³ ASTM D792 / ASTM D1505 Tensile Stress at Yield (Tensile strength) 22 MPa ASTM F648 / ASTM D638 Tensile Stress at Break (Ultimate tensile strength) 58 MPa ASTM F648 / ASTM D638 Elongation (at Break) 450.0 % ASTM F648 / ASTM D638 Shore Hardness (15 sec) 66.0 D - Scale ASTM D2240 Notched Impact Strength (Charpy) 196 kJ/m² ISO 11542.2 Crystallinity (1ˢᵗ heat, 20°C - 160°C) 59.0 % ASTM F2625, Differential Scanning Calorimeter Notched Impact Strength (lzod) 144 kJ/m² ASTM F648 Water Absorption (at 23°C until Saturation) max. 0.05 % ASTM D570 - Thermal Properties
Value Units Test Method / Conditions Melting Temperature (10°C/min) 136.0 °C ASTM DF2625, Differential Scanning Calorimeter Vicat Softening Point (10N, at 50°C/hr) 134.0 °C ASTM D1525 Coefficient of Linear Thermal Expansion (23°C to 80°C) 1.8 x 10⁻⁴ K⁻¹ ASTM D696 Heat Deflection Temperature (at 1.8 MPa) 42.0 °C ASTM D648 Thermal Conductivity approx. 0.4 W/(m*K) DIN 52612 Crystallization Temperature Range (20°C - 160°C) 126 - 144 °C ASTM F2625 Ash Particles max. 150 mg/kg ISO 3451 -1 Oxidation Resistance (Surface oxidation index) max. 0.1 ASTM F2102 Oxidation Resistance (Bulk oxidation index) max. 0.1 ASTM F2102 Oxidation Induction Time to Conducted (at 200°C) 10 min ASTM D3895
Regulatory & Compliance
- Quality Standards