Line Call Out | F712112B3E12K6M8 | - | ASTM F104 |
Compressibility (1/32") | 6 - 12 | % | ASTM F36J |
Creep relaxation (1/32") | 20 | % | ASTM F38B |
Density | 131 | lb/ft ³ (2.1 g/cc ³) | ASTM D149-95a |
Dielectric Strength | 10 | kV/mm | ASTM D149-95a |
KLINGER Hot Compression Test Thickness Decrease 572°F (23°C) additional | 6 | % | - |
KLINGER Hot Compression Test Thickness Decrease 73°F (23°C) initial | 10 | % | - |
Leachable Chloride Content | 150 | ppm | FSA Method |
Recovery | 50 | % | ASTM F36J |
Thickness Increase ASTM F146 after immersion in ASTM Fuel A, 5h/73°F (23°C) | 0 - 5 | % | - |
Thickness Increase ASTM F146 after immersion in ASTM Fuel B, 5h/73°F (23°C) | 0 - 5 | % | - |
Thickness Increase ASTM F146 after immersion in ASTM Oil IRM 901, 5h/300°F (149°C) | 0 - 5 | % | - |
Thickness Increase ASTM F146 after immersion in ASTM Oil IRM 903, 5h/300°F (149°C) | 5 - 10 | % | - |
Weight increase ASTM F146 after immersion in Fuel B, 5h/73°F (23°C) | max. 9 | % | - |