Enhanced TDS
Knowde-enriched technical product data sheet
Identification & Functionality
- Polymer Name
- Technologies
- Product Families
Features & Benefits
- Materials Features
Applications & Uses
- Markets
- Applications
- Plastics & Elastomers End Uses
- Typical Applications
Oil resistant tube, hose, packing, etc., replacement of NBR rubbers
Properties
- Typical Properties
Value Units Test Method / Conditions Aging Test CH 120℃×200hrs -6 - - Aging Test Sc(EB) 120℃×200hrs 4 % - Aging Test Sc(TB) 120℃×200hrs 20 % - Brittle Temperature 3 ℃ - CS 70℃×22hrs 112 % - Density 1 g/cm3 - Elongation at 100% 9 MPa - Elongation at break -36 % - Hardness (15sec) 86 - - MFR 230℃×98N 5.7 g/10min - Oil resistance △V 120℃×70hrs -1 % IRM903 Oil resistance △V 23℃×70hrs -9 % Fuel-C Oil resistance CH 120℃×70hrs -45 - IRM903 Oil resistance CH 23℃×70hrs -36 - Fuel-C Oil resistance Sc(EB) 120℃×70hrs -29 % IRM903 Oil resistance Sc(EB) 23℃×70hrs -36 % Fuel-C Oil resistance Sc(TB) 120℃×70hrs 41 % IRM903 Oil resistance Sc(TB) 23℃×70hrs -4 % Fuel-C Tensile Strength 240 MPa -