E-Glass 1142

E-glass 1142 is also known as electrical glass—is the standard glass composition used for most glass fibers. It is made from the oxides of silicon, aluminum, calcium, magnesium, and boron.

Brand: E-Glass (8 products)

Reinforcement Material: Glass Fibers

Reinforcement Form: Plain Weave Fabric

Features: Chemical Resistance, Chemical Resistant, Cost Effective, Dimensional Stability, Ease of Handling, Easy Handling, Electrically Insulating, Excellent Mechanical Strength, Good Electrical Properties, Good Thermal Stability, Heat Resistance, High Stiffness, High Strength, Improved Dimensional Stability, Thermal Stability

Enhanced TDS

Knowde-enriched technical product data sheet

Identification & Functionality

Chemical Family
Reinforcement Form
Reinforcement Material
Composite Materials Functions
Technologies
Product Families

Features & Benefits

Materials Features
Characteristics of E-Glass

E-fiberglass is more commonly used in the fiber-reinforced polymer composite industry. It offers a good balance between performance and cost, demonstrating excellent strength and stiffness (although not as good as S-glass) as well as good resistance to chemicals, moisture, and heat. Since it was developed specifically for use in electrical applications, one of its key characteristics is its ability to insulate electricity. In addition to electrical components, other typical uses for the material include aerospace and other industrial equipment components (e.g., heat shields), marine and other recreational equipment (e.g., surfboards), and general industrial components (e.g., awnings, belts, and gaskets).

E-glass is available in a variety of weave patterns. Some of the best patterns for the fabric are:

  • Plain weave: consists of fibers interlaced in an alternating over/under pattern
  • Twill: consists of warp fibers floating over two consecutive fill fibers

Applications & Uses

Properties

Physical Form
Mechanical Properties
ValueUnitsTest Method / Conditions
Density2.54g/cm3-
Tensile Strength3400MPa-
Modulus of Elasticity72GPa-
Percent Elongation4.7--