Enhanced TDS
Knowde-enriched technical product data sheet
Identification & Functionality
- Chemical Family
- Polymer Name
- Reinforcement Material
- Composite Materials Functions
- Plastics & Elastomers Functions
- Technologies
- Product Families
Features & Benefits
- Labeling Claims
- Materials Features
Applications & Uses
- Markets
- Applications
- Plastics & Elastomers End Uses
- Plastics & Elastomers Processing Methods
- General Processing Recommendations
Green Dot’s Terratek® WC200180 resin needs to be dried before processing if the moisture is above 0.5%. Resin will dry quickly at 150°F in a desiccant dryer. Avoid prolonged resin exposure to air during molding or storage as the material can pick up moisture.
For best molding results, larger gates and runners are recommended. The injection pressure required to fill the mold is much higher than typical injection molding grade plastics. Typical injection molding temperatures are listed below, these are only a guide and may need to be changed based on the particular application :
Rear 350°F to 360°F Middle 350°F to 360°F Front 360°F to 375°F Nozzle 360°F to 375°F Mold 60°F to 170°F The melt temperature of the resin should remain below 400°F to prevent the material from discoloring and having a burnt odor.
Properties
- Physical Form
- Typical Properties
Value Units Test Method / Conditions Specific Gravity 1.19 g/cm³ ASTM D792 Shrinkage 0.006 in/in - Melt Index 3.2 g/10 min ASTM D1238 Flex Strength 18035 psi ASTM D790 Flex Modulus 579702 psi ASTM D790 Tensile Strength 10522 psi ASTM D638 Tensile Modulus 693140 psi ASTM D638 Elongation 2.08 % - Notched Izod 0.67 ft lb/in ASTM D256
Packaging & Availability
- Packaging Type
- Packaging
Terratek® WC200180 resin is typically packaged in a sealed plastic-lined Gaylord at 1200 lbs/Gaylord.
Storage & Handling
- Storing
The product should be stored in a cool, dry, and sanitary area to achieve maximum stability.