Value Units Test Method / Conditions Specific gravity 1.07 - ASTM D792 Hardness 78 Shore A ASTM D2240 Tensile strength 90 kgf/cm2 ASTM D412 Elongation at Break 500 % ASTM D412 Melt Index G7 g/10min ASTM D1238 ABS Adhesion 12 kgf/2.5cm HT Method PC Adhesion 12 kgf/2.5cm HT Method Brittle Temperature -40 °C Estimate Shrinkage (Reference Only) 0.7 % Machine Direction Shrinkage (Reference Only) 0.9 % Transverse Direction
Regulatory & Compliance
Technical Details & Test Data
- HAR Series Properties/Injection Molding Information
Injection Molding Most olefin plastic machines can be used for injection molding Compression Ratio 2.4 and higher Cylinder Temperature (Feed Zone) 180-190 °C Cylinder Temperature (Center Zone) 185-200 °C Cylinder Temperature (Front Zone) 195-205 °C Cylinder Temperature (Nozzle) 200-220 °C Mold Temperature 30-50 °C Injection Pressure 30-50 kg/cm2 Injection Rate Moderate Hold Time 5 sec. Screw Speed Medium Back Pressure 5-10 kg/cm2 Cycle Time (Goods material thickness under 2 mm) 15-30 sec. Please adjust the injection molding temperature based on the product size and mold structure around 180 °C to 220 °C during processing, but not exceeding 240 °C.