Enhanced TDS
Knowde-enriched technical product data sheet
Identification & Functionality
- Core Type
- Composite Materials Functions
- Technologies
- Product Families
Features & Benefits
- Labeling Claims
- Materials Features
- Product Highlights
- Superior fire retardancy (FAR 25.853; EN 45545, EN 13501)
- Outstanding fatigue strength
- Excellent long term thermal stability up to 100 °C (212 °F)
- Best thermal stability in process up to 150 °C (302 °F)
- Good thermal insulation
- Highly consistent material properties
- Easy to process with all types of resin and lamination processes
- Good adhesion (skin-to-core bond)
- Very high chemical stability
- No water absorption, no after-expansion, no outgassing
Applications & Uses
- Markets
- Applications
- Composites Processing Methods
- Application
- Aerospace: Interiors, galleys, meal trolleys, radomes
- Road and Rail: Floors, sidewalls, front ends, interiors, roofs, engine covers
- Marine: Decks, interiors, superstructures
- Industrial: Covers, containers, x-ray tables, sporting goods
- Architecture and Construction: Roofs, claddings, domes, portable building
- Processing
- Contact molding (hand/spray)
- Vacuum infusion
- Resin infusion / injection (VARTM / RTM)
- Adhesive bonding
- Pre-preg processing
- Compression molding (GMT, SMC)
- Thermoforming
Properties
- Mechanical Properties
Value Units Test Method / Conditions Compressive Strength Perpendicular to the Plane 1.4 (203) N/mm² (psi) - Compressive Modulus Perpendicular to the Plane 80 (11,600) N/mm² (psi) - Tensile Strength Perpendicular to the Plane 2.2 (319) N/mm² (psi) - Tensile Modulus Perpendicular to the Plane 120 (17,400) N/mm² (psi) - Shear Strength 0.8 (116) N/mm² (psi) - Shear Modulus 20 (2,900) N/mm² (psi) - Shear Elongation at Break 10.0 % - - Typical Properties
Value Units Test Method / Conditions Standard Sheet Length 2440 (96) mm ± 5 (in ± 0.2) - Standard Sheet Width 1220 (48) mm ± 5 (in ± 0.2) - Standard Sheet Thickness 5 to 100 (⅛ to 4) mm ± 0.5 (in ± 0.02) - Density 110 (6.8) kg/m³ (lb/ft³) - Thermal Conductivity at 10°C 0.035 (0.243) W/m.K (BTU.in/ft2.hr.°F) -