MOCOM Compounds ALCOM® MED PS 2015 05001 is an injection molding grade material suitable for producing housings used in various applications. It is composed of impact polystyrene as the base polymer and 15% glass fibers as the filler/additive system. This material should be stored in a dry, protected location away from light, and not above 30°C.

Polymer Name: Polystyrene (unspecified)

Fillers Included: Glass Fiber, Milled Glass Fiber

Processing Methods: Injection Molding

Technical Data Sheet
Message our experts with questions
Lonnie Tough Jr avatar

Lonnie Tough Jr

Sales

I support all stages of Business Development, from concept, to design, tooling, manufacturing, processing, and material selection.

Blaine Priebe avatar

Blaine Priebe

R&D

Please reach out to me with any questions, I am happy to assist you in finding the right product or learning more about our storefront

Jack Chiang avatar

Jack Chiang

Sales

With 22 Years of compounding experience I have the knowledge in resin selection and filler technology to be your material expert in any market segment

Salvador Ramiro Gonzalez Vaca avatar

Salvador Ramiro Gonzalez Vaca

Business Development Manager

As an expert in plastics with 10 years of experience and certified as a Master Molder, I can support you in all stages of Business Development.

MN

Mike Najjar

Business Development

Please reach out to me with any questions, I am happy to assist you in finding the right product or learning more about our storefront

Knowde Enhanced TDS

Identification & Functionality

Chemical Family
Plastics & Elastomers Functions
Technologies

Features & Benefits

Materials Features

Applications & Uses

Plastics & Elastomers End Uses
Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Flexural Modulus4600.0MPaISO 178
Flexural Strength52.0MPaISO 178
Tensile Modulus4300.0MPaISO 527
Tensile Stress at Yield25.0MPaISO 527
Tensile Elongation at Yield0.9%ISO 527
Tensile Elongation at Break6.7%ISO 527
Impact Strength (Charpy, at 23°C)13.0kJ/m²ISO 179/1eU
Impact Strength (Charpy, at -40°C)12.0kJ/m²ISO 179/1eU
Notched Impact Strength (Charpy, at 23°C)3.5kJ/m²ISO 179/1eA
Notched Impact (Charpy, at -40°C)1.5kJ/m²ISO 179/1eA
Physical Properties
ValueUnitsTest Method / Conditions
Density1210.0kg/m³ISO 1183
Thermal Properties
ValueUnitsTest Method / Conditions
Vicat B5089.0°CISO 306
HDT / A (1.8 MPa)83.0°CISO 75-1/-2
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Mould Temperature10 - 70°C-
Melt Temperature180 - 260°C-
Rheological Properties
ValueUnitsTest Method / Conditions
Melt Index (MVR)6.0cm³/10minISO 1133
MVR Temperature200.0°C-
MVR Load5.0kg-
Shrinkage (24h)0.1 - 0.5%ISO 294-4

Regulatory & Compliance

Technical Details & Test Data

Pre-Drying Conditions
  • In a dry air (dessiccant) dryer 60-80 °C for 2-3 h
  • In an air circulatIng dryer 60-80 °C for 2-3 h
  • Dependant on moisture content

Storage & Handling

Storage Conditions

Store in dry, protected from light not above 30°C.